| Наименование |
Контракт |
Склад |
|
Cotton pulp
|
Call
|
Call
|
COTTON CELLULOSE
|
Items
|
Norm
|
|
1st sort
|
2nd sort
|
|
α-the cellulose content %≥
|
|
|
|
a) mass-method
|
for 25, 35 - 97,7
for other - 98,0
|
97,5
|
|
б) photometric method
|
для марок 25, 35 - 97,7
для других - 98,0
|
97,5
|
|
the degree of moisture-absorbing, g min
|
140
|
130
|
|
water content, % max
|
10,0
|
|
ash content, % max
|
0,2
|
0,3
|
|
contents of the things that don't dissolve in sulphuric acid
, % max
|
0,30
|
0,50
|
|
dust content, % max
|
0,2
|
|
Whiteness, % min
|
85
|
-
|
|
Fe, mg/kg of waterless cellulose, max
|
-
|
|
the viscosity mPa sec for marks
|
|
15
|
1,0-2,0 (10-20)
|
|
25
|
2,1-3,0 (21-30)
|
|
35
|
3,1-4,5 (31-45)
|
|
70
|
4,6-8,5 (46-85)
|
|
100
|
8,6-11,5 (86-115)
|
|
150
|
11,6-17,5 (116-175)
|
|
250
|
17,6-30,0 (176-300)
|
|
350
|
30,1-43,0 (301-430)
|
|
650
|
43,1-85,0 (431-850)
|
Call +7 (812) 327-27-76 (multichannel)